We always focus on the Cr5MoV Cold Work Die Steel, SKH51 High Speed Steel, Unhardened steel plate industry, actively seek model innovation and management breakthroughs, and constantly improve our comprehensive strength and competitive advantage. After years of development and exploration of Cold Hardening Steel, we have accumulated rich technology and experience to create high quality products. All along, we uphold the spirit of loyalty, unity, hard work and innovation, and take diligence, integrity, hard work, innovation and win-win as our core values. We insists on both quality and environmental protection. Since its establishment, the company has resolutely won a good reputation from customers with its exquisite appearance design, serious and pragmatic work spirit, and good and thoughtful follow-up services. With years of experience, we have become a trusted name in the industry. We only find ways to succeed, not to find reasons for failure, and ultimately make the impossible possible.
  • Cold Hardening Steel
    Product Model: 9Mn2V
    Chemical Composition (Range): C≈0.85–0.95%, Mn≈1.7–2.0%, V≈0.1–0.25%
    Quenched Hardness: 58 – 62HRC
    Recommended Quenching Temperature: 780°C –...
  • SKH51 High Speed Steel
    Chemical Composition (Typical): C≈0.83%, W≈6.4%, Mo≈5%, Cr≈4%, V≈1.9%
    Delivery Hardness: Annealed ≤248HB
    Quenched Hardness: 62 – 67HRC
    Hardness After High-Temperature Tempering:...
  • SKH-9 High Speed Steel
    Chemical Composition (Typical): C≈0.85%, W≈6%, Mo≈5.2%, Cr≈4.1%, V≈2%
    Hardness After Quenching & Tempering: 63 – 68HRC
    Recommended Quenching Temperature: 1180°C –...
  • Cold Work Mold Steel
    Product Model: CrWMn
    Chemical Composition (Range): C≈0.9–1.05%, Cr≈0.9–1.2%, W≈1.2–1.6%, Mn≈0.8–1.1%
    Delivery Hardness: Annealed ≤207HB
    Quenched Hardness: 60 –...
  • Cold Work Alloy Steel
    Product Model: 9CrSi
    Chemical Composition (Range): C≈0.85–0.95%, Cr≈0.95–1.25%, Si≈1.2–1.6%, Mn≈0.3–0.6%
    Quenched Hardness: 60 – 63HRC
    Recommended Quenching Temperature: 830°C –...
  • Cold Work Tooling Steel
    Product Model: Cr12MoV
    Chemical Composition (Range): C≈1.45–1.7%, Cr≈11–12.5%, Mo≈0.4–0.6%, V≈0.15–0.3%
    Hardness After Quenching & Tempering: 58 – 62HRC
    Recommended Quenching...
  • Cr5MoV Cold Work Die Steel
    Product Model: Cr5MoV
    Chemical Composition (Range): C≈0.95–1.05%, Cr≈4.75–5.5%, Mo≈0.4–0.6%, V≈0.2–0.3%
    Quenched Hardness: 59 – 63HRC
    Recommended Quenching Temperature: 940°C –...
  • DC53 Cold Work Tool Steel
    Product Model: DC53
    Chemical Composition (Typical): C≈1.0%, Cr≈8%, Mo≈2%, V≈0.3%
    Low-Temperature Tempering Hardness: 58 – 62HRC
    High-Temperature Tempering Hardness: 62 –...
  • Cold Work Tool Steel
    Product Model: T8A
    Chemical Composition (Range): C≈0.75–0.84%
    Quenched Hardness: 60 – 62HRC
    Recommended Quenching Temperature: 780°C – 800°C
    Recommended Tempering...
  • Cold Work Die Steel
    Product Model: T10A
    Chemical Composition (Range): C≈0.95–1.04%
    Quenched Hardness: 61 – 63HRC
    Recommended Quenching Temperature: 770°C – 790°C
    Recommended Tempering...
  • High Toughness Cold Work Tool Steel
    Product Model: T12A
    Chemical Composition (Range): C≈1.15–1.24%
    Quenched Hardness: 62 – 64HRC
    Recommended Quenching Temperature: 760°C – 780°C
    Recommended Tempering...
  • SKS3 Cold Work Die Steel
    Product Model: SKS3
    Chemical Composition (Typical): C≈0.95%, Cr≈0.5%, W≈0.5%
    Quenched Hardness: 60 – 63HRC
    Recommended Quenching Temperature: 800°C – 830°C
    Quenching...
Linda Moon star star star star star
Managers can always find small problems in production at the first time and solve them immediately. This is a manifestation of professionalism. It was the right choice to choose this company!
Dorothea Daniels star star star star star
"Integrity" and "friendliness" are the highest praise we can give you.
John Yarbro star star star star star
Generally speaking, the company has practiced the concept of customer service and has been solving various problems for us.
David McPherson star star star star star
Their product is very good, beautiful and functional, I plan to buy another one.
Jordan Williams star star star star star
The price of their products is not forced, which is good.
Wesley Gustin star star star star star
The first time I bought a product I was satisfied with online shopping, thank you!
Our company has been committed to the design and manufacture of plastic mold steel, extrusion mold steel since its establishment. Now it has a large number of excellent engineers and technicians and a perfect management system and has become a comprehensive company integrating design, manufacture, and engineering implementation. entity. And our products have been sold well in many regions at home and abroad. We are one of the most professional cold hardening steel manufacturers and suppliers in China, also support customized service. Please feel free to wholesale high quality cold hardening steel in stock here from our factory. Also, pricelist is available.
Send Inquiry