Cold Work Mold SteelProduct Model: CrWMn
Chemical Composition (Range): C≈0.9–1.05%, Cr≈0.9–1.2%, W≈1.2–1.6%, Mn≈0.8–1.1%
Delivery Hardness: Annealed ≤207HB
Quenched Hardness: 60 –... -
D2 Cold Work Tool SteelChemical Composition (Typical): C≈1.55%, Cr≈12%, Mo≈0.95%, V≈0.9%
Delivery Hardness: Annealed ≤255HB
Hardness After Quenching & Tempering: 58 – 62HRC
Recommended Quenching... -
SKH51 High Speed SteelChemical Composition (Typical): C≈0.83%, W≈6.4%, Mo≈5%, Cr≈4%, V≈1.9%
Delivery Hardness: Annealed ≤248HB
Quenched Hardness: 62 – 67HRC
Hardness After High-Temperature Tempering:... -
SKH-9 High Speed SteelChemical Composition (Typical): C≈0.85%, W≈6%, Mo≈5.2%, Cr≈4.1%, V≈2%
Hardness After Quenching & Tempering: 63 – 68HRC
Recommended Quenching Temperature: 1180°C –... -
Cold Work Alloy SteelProduct Model: 9CrSi
Chemical Composition (Range): C≈0.85–0.95%, Cr≈0.95–1.25%, Si≈1.2–1.6%, Mn≈0.3–0.6%
Quenched Hardness: 60 – 63HRC
Recommended Quenching Temperature: 830°C –... -
Cold Hardening SteelProduct Model: 9Mn2V
Chemical Composition (Range): C≈0.85–0.95%, Mn≈1.7–2.0%, V≈0.1–0.25%
Quenched Hardness: 58 – 62HRC
Recommended Quenching Temperature: 780°C –... -
Cr5MoV Cold Work Die SteelProduct Model: Cr5MoV
Chemical Composition (Range): C≈0.95–1.05%, Cr≈4.75–5.5%, Mo≈0.4–0.6%, V≈0.2–0.3%
Quenched Hardness: 59 – 63HRC
Recommended Quenching Temperature: 940°C –... -
SKD11 Cold Work Die SteelProduct Model: SKD11
Chemical Composition (Typical): C≈1.4%, Cr≈11.5%, Mo≈0.8%, V≈0.3%
Hardness After Quenching & Tempering: 58 – 62HRC
Recommended Quenching Temperature:... -
DC53 Cold Work Tool SteelProduct Model: DC53
Chemical Composition (Typical): C≈1.0%, Cr≈8%, Mo≈2%, V≈0.3%
Low-Temperature Tempering Hardness: 58 – 62HRC
High-Temperature Tempering Hardness: 62 –... -
Cold Work Die SteelProduct Model: T10A
Chemical Composition (Range): C≈0.95–1.04%
Quenched Hardness: 61 – 63HRC
Recommended Quenching Temperature: 770°C – 790°C
Recommended Tempering... -
High Toughness Cold Work Tool SteelProduct Model: T12A
Chemical Composition (Range): C≈1.15–1.24%
Quenched Hardness: 62 – 64HRC
Recommended Quenching Temperature: 760°C – 780°C
Recommended Tempering... -
SKS3 Cold Work Die SteelProduct Model: SKS3
Chemical Composition (Typical): C≈0.95%, Cr≈0.5%, W≈0.5%
Quenched Hardness: 60 – 63HRC
Recommended Quenching Temperature: 800°C – 830°C
Quenching...
webNov 15, 2016 · Area ablation of Cr12MoV cold-work mold steel was carried out using a picosecond (ps) pulse Nd:YVO 4 laser. The effects of laser fluence and wavelength on the ablation rate and...
webDiscover our wide range of hot work steel, cold work steel and plastic molding steel grades. Working with the right tool steel is key to guarantee a high productivity and reliability in production...
webThe low-alloy cold work mold steel, such as 9CrWMn, is typically used for simple molds in small batch production. It’s also used for prototype molds that endure minimal impact. On the other hand,...
webCold heading mould, deep drawing mould, cold extrusion mould. Thermosetting resin type touch, general plastic mold. SKD11 is a general cold work die steel with high wear...
webHeat Treatment of 1.2358 Cold Work Steel. Softening annealing at 820 – 860°C. Stress relief annealing at 600 – 650°C. Hardening at 950-970°C with cooling in oil or salt bath. Tempering at...
webJul 16, 2021 · D2 steel is a high carbon – high chromium air hardening cold work tool steel, heat treatable to 60-62 HRC. D2 offers excellent wear and abrasion resistance, due to large volumes of...