SKD6 Tool SteelProduct Model: SKD6
Material Type: Cr-Mo-V series medium-temperature hot work steel
Tempering Hardness: 44 – 50HRC
Key Features: Good machinability; excellent welding... -
H13 Hot Work Tool SteelProduct Model: H13
Chemical Composition (Typical): C≈0.4%, Cr≈5.2%, Mo≈1.3%, V≈1.0%
Delivery Hardness: Annealed ≤229HB
Hardness After Quenching & Tempering: 48 –... -
Hot Die SteelProduct Model: GHD-12344
Chemical Composition (Typical): C≈0.38%, Cr≈5.0%, Mo≈1.3%, V≈0.9%
Tempering Hardness: 46 – 52HRC
Recommended Quenching Temperature:... -
SKD61 Tool SteelParameter: Value / Description
Product Model: SKD61
Chemical Composition (Typical): C≈0.35%, Cr≈5.0%, Mo≈1.2%, V≈1.0%
Hardness Range: 47 – 53HRC
Recommended Quenching... -
Hot Work Die SteelProduct Model: 3Cr2W8V
Chemical Composition (Typical): C≈0.3%, Cr≈2.5%, W≈8%, V≈0.4%
Tempering Hardness: 48 – 54HRC
Recommended Quenching Temperature: 1080°C –... -
1.2888 Tool SteelProduct Model: GHD-12888
Chemical Composition (Typical): C≈0.33%, Cr≈3.2%, W≈8.3%, V≈0.4%
Tempering Hardness: 49 – 55HRC
Key Features: High-temperature red hardness; high... -
H11 Die SteelProduct Model: GHD-H11
Chemical Composition (Typical): C≈0.35%, Cr≈5.0%, Mo≈1.4%, V≈0.4%
Hardness Range: 45 – 50HRC
Recommended Quenching Temperature: 1010°C
Recommended... -
SKD5 Tool SteelProduct Model: SKD5
Chemical Composition: Tungsten-type hot work steel (Improved grade comparable to 3Cr2W8V)
Tempering Hardness: 47 – 53HRC
Key Features: Excellent... -
Hot Work SteelProduct Model: 4Cr5MoSiV1
Chemical Composition (Range): C≈0.32–0.42%, Cr≈4.75–5.5%, Mo≈1.1–1.5%, V≈0.8–1.2%
Hardness Range: 46 – 52HRC
Key Features: General-purpose hot work...
H-13 is a tool steel alloy that contains chromium, molybdenum, and vanadium. The molybdenum and vanadium provide the strength in this grade while the chromium aids in softening the...
Grade Summary: Tool Steel H13 is a chromium, molybdenum, vanadium hot work tool steel which is has high hardenability and excellent toughness, this is due to the fact that the material contains...
Steel H13 is a Tool Steel (High-alloy steel) that has on top of the 0.4% of carbon an additional 8.2% of manganese, chromium, nickel, and molybdenum. (See details in the below table ). Steel H13 has...
20-40 CFH. Description: WT H-13 is often used for welding hot work tool steels with good heat checking resistance, hot tensile properties, as well as high wear resistance. It is often used in dies,...
H13 tool steel heat treatment including: Annealing Heat uniformly to 845 to 900 °C (1550 to 1650 °F) in a controlled atmosphere furnace, or place the part in a neutral compound to prevent...
Double tempering is recommended for the H-13 grade. For most applications, H-13 should be tempered in the 1100° F - 1150° F range. The above tempering table may be used as a guide. However, since...